Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ALIMEX 6082 T651 Aluminum Alloy Rolled

Category Metal , Nonferrous Metal , Aluminum Alloy , 6000 Series Aluminum Alloy
Manufacturer ALIMEX GmbH
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ALIMEX 6082 T651 Aluminum Alloy Rolled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Rolled aluminium material according to DIN EN standard. Information provided by ALIMEX GmbHSolution heat treated, stress relieved by stretching a controlled amount and then artificially aged.
Physical Properties Metric English Comments
Density 2.70 g/cc
0.0975 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell >= 85
>= 85
Tensile Strength, Ultimate >= 275 MPa
>= 39900 psi
Rm
Tensile Strength, Yield >= 240 MPa

@Strain 0.200 %
>= 34800 psi

@Strain 0.200 %
Elongation at Break 6.0 - 9.0 %
6.0 - 9.0 %
Modulus of Elasticity 70.0 GPa
10200 ksi
Thermal Properties Metric English Comments
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 °C
13.0 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 170.0 - 220.0 W/m-K
1180 - 1527 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000313 - 0.00000417 ohm-cm
0.00000313 - 0.00000417 ohm-cm
Descriptive Properties Value Comments
Corrosion Resistance Good
Machinability Good
Protective Anodizing Very good, not decorative
Welding Properties (WIG, MIG) Good
Users viewing this material also viewed the following: