Material Notes:
BC 5010 is a high quality, low viscosity room temperature curing laminating resin. A Safety System for the production of a variety of dimensionally stable fiberglass tools. BC 5010 features low odor and rapid “wet-out” with no vertical drain off. An excellent general purpose laminating resin to meet the tooling requirements for automotive, aircraft and foundry.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
Brookfield Viscosity 3200 cP

@Temperature 25.0 °C
3200 cP

@Temperature 77.0 °F
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore D 90

@Temperature 25.0 °C
90

@Temperature 77.0 °F
Tensile Strength, Ultimate 173 MPa
25100 psi
Flexural Strength 210 MPa
30500 psi
Flexural Modulus 13.0 GPa
1880 ksi
Compressive Strength 266 MPa
38600 psi
Thermal Properties Metric English Comments
CTE, linear 23.4 µm/m-°C
13.0 µin/in-°F
Deflection Temperature at 1.8 MPa (264 psi) 87.8 °C
190 °F
Processing Properties Metric English Comments
Cure Time 480 - 720 min

@Temperature 24.0 °C
8.00 - 12.0 hour

@Temperature 75.2 °F
Pot Life 25 - 30 min

@Temperature 24.0 °C
25 - 30 min

@Temperature 75.2 °F
1 lb. mass
Descriptive Properties Value Comments
Mix Ratio 6:1 by weight, 4.5:1 by volume, resin/harder