Material Notes:
Aluminium rolled plates which have been machined on both sides. Has a precise surface finish and high tensile strength. The temper values and the material conditions are not changed by surface-machining and clearing away of the rolled surface on both sides.Information provided by ALIMEX GmbHSolution heat-treated, stress-relieved by stretching a controlled amount and then artificially aged.
Physical Properties Metric English Comments
Density 2.68 g/cc
0.0970 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell >= 89
>= 89
Tensile Strength, Ultimate >= 295 MPa
>= 42800 psi
Rm
Tensile Strength, Yield >= 240 MPa

@Strain 0.200 %
>= 34800 psi

@Strain 0.200 %
Elongation at Break <= 8.0 %
<= 8.0 %
Modulus of Elasticity 70.0 GPa
10200 ksi
Thermal Properties Metric English Comments
CTE, linear 23.4 µm/m-°C

@Temperature 20.0 °C
13.0 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 170.0 - 220.0 W/m-K
1180 - 1527 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000313 - 0.00000417 ohm-cm
0.00000313 - 0.00000417 ohm-cm
Descriptive Properties Value Comments
Machinability Good
Protective Anodizing Very good, not decorative
Welding Properties (WIG, MIG) Good