Victrex® PEEK 600PF Polyetheretherketone  (discontinued **)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Unreinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Victrex® PEEK 600PF Polyetheretherketone  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression compounding, low flow, FDA food contact compliantInformation provided by Victrex
Physical Properties Metric English Comments
Bulk Density 0.250 g/cc
0.00903 lb/in³
ISO 1183
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183
Particle Size 70 µm
70 µm
D<sub>50</sub>; ISO 13320-1
Viscosity 450000 cP

@Temperature 400 °C
450000 cP

@Temperature 752 °F
Melt; ISO 11443
Mechanical Properties Metric English Comments
Tensile Strength, Yield 90.0 MPa
13100 psi
Result based on similar products; ISO 527
Elongation at Break 30 %
30 %
Result based on similar products; ISO 527
Tensile Modulus 3.70 GPa
537 ksi
Result based on similar products; ISO 527
Flexural Strength 150 MPa
21800 psi
Result based on similar products; ISO 178
Flexural Modulus 4.10 GPa
595 ksi
Result based on similar products; ISO 178
Izod Impact, Notched (ISO) 7.50 kJ/m²
3.57 ft-lb/in²
Result based on similar products; ISO 180/A
Izod Impact, Unnotched (ISO) NB
NB
Result based on similar products; ISO 180/U
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
ISO 11357
Glass Transition Temp, Tg 143 °C
289 °F
Onset; ISO 11357
Processing Properties Metric English Comments
Processing Temperature 380 - 400 °C
716 - 752 °F
Dry Time 3 hour

@Temperature 150 °C
3 hour

@Temperature 302 °F
5 hour

@Temperature 120 °C
5 hour

@Temperature 248 °F
Descriptive Properties Value Comments
Color Natural