Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Victrex® PEEK 650P PolyEtherEtherKetone

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, Unreinforced
Manufacturer Victrex
Trade Name PEEK
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Victrex® PEEK 650P PolyEtherEtherKetone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, coarse powder for extrusion compounding, low flow, FDA food contact compliant, color natural.Information Provided by VICTREX®
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183
Viscosity 500000 cP

@Temperature 400 °C
500000 cP

@Temperature 752 °F
melt; ISO 11443
Mechanical Properties Metric English Comments
Tensile Strength, Yield 90.0 MPa
13100 psi
ISO 527
Elongation at Break 30 %
30 %
ISO 527
Tensile Modulus 3.90 GPa
566 ksi
ISO 527
Flexural Strength 150 MPa
21800 psi
ISO 178
Flexural Modulus 3.60 GPa
522 ksi
ISO 178
Izod Impact, Notched (ISO) 7.50 kJ/m²
3.57 ft-lb/in²
ISO 180/A
Izod Impact, Unnotched (ISO) NB
NB
ISO 180/U
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
ISO 11357
Glass Transition Temp, Tg >= 143 °C
>= 289 °F
Onset; ISO 11357
150 °C
302 °F
Midpoint; ISO 11357
Processing Properties Metric English Comments
Processing Temperature 380 - 400 °C
716 - 752 °F
Dry Time 3.00 hour

@Temperature 150 °C
3.00 hour

@Temperature 302 °F
5.00 hour

@Temperature 120 °C
5.00 hour

@Temperature 248 °F
Copyright © lookpolymers.com All Rights Reserved