Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melting Point = 219 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 219 °C
426 °F
ASTM D789
NYCOA 1417HS PA 6
impact modified, heat stabilized, medium high impact strengthInformation provided by NYCOA, Inc.
Melting Point 219 °C
426 °F
Oxford Polymers Oxnilon 6-14GF 14% Glass Fiber Filled Nylon 6 for Injection Molding
14% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers.
Melting Point 219 °C
426 °F
Oxford Polymers Oxnilon 6-33GF 33% Glass Fiber Filled Nylon 6 for Injection Molding
33% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers.
Melting Point 219 °C
426 °F
Oxford Polymers Oxnilon 6-43GF 43% Glass Fiber Filled Nylon 6 for Injection Molding
43% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers.
Melting Point 219 °C
426 °F
10°C/min; DAM; ISO 11357-1/-3
DuPont Performance Polymers Zytel® 73G50HSLA BK416 Nylon 6  (Unverified Data**)
Zytel® 73G50HSLA BK416 is a 50% glass fiber reinforced, heat stabilized, lubricated, polyamide 6 resin for injection molding. It has an excellent surface appearance and gloss.Information provided ..
Melting Point 219 °C
426 °F
Peak
LG Chemical KEYFLEX BT 1072D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical
Melting Point 219 °C
426 °F
10°C/min; ISO 11357-1, -3
Lanxess Durethan® BC 550 Z DUSXBL 900116 Nylon 6, Impact Modified
PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Melting Point 219 °C
426 °F
10°C/min; ISO 11357-1, -3
Lanxess Durethan® BC 600 HTS DUSXBL 900116 Nylon 6, Impact Modified
PA 6, non-reinforced, extrusion, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Melting Point 219 °C
426 °F
10°C/min; ISO 11357-1, -3
Lanxess Durethan® BKV 215 H2.0 DUS008 901510 Nylon 6, Impact Modified
PA 6, 15% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Melting Point 219 °C
426 °F
10°C/min; ISO 11357-1/-3
Lanxess Durethan® TP 140-009 901510 Nylon 6, 15% Glass Fiber
PA 6 extrusion- and blow molding-grade, 15% glass fibers, elastomer-modified, good heat-ageing resistance, dry-impact modified
Melting Point 219 °C
426 °F
10°C/min; ISO 11357-1, -3
Lanxess Durethan® BKV 30 G W1 901317 Nylon 6, Glass Fiber Reinforced
PA 6, 30% glass fibers, injection molding, weather stabilizedInformation provided by LANXESS.
Melting Point 219 °C
426 °F
10°C/min; ISO 11357-1, -3
Lanxess Durethan® BKV 30 H2.0 EF 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS.
Melting Point 219 °C
426 °F
10°C/min; ISO 11357-1/-3
Lanxess Durethan® BKV 315 Z H2.0 901510 Nylon 6, 15% Glass Fiber
PA 6 extrusion- and blow molding-grade with 15% glass fibers, branched/structural viscosity, elastomer-modified, good heat-ageing resistance, dry-impact modifiedApplication Examples: air intake hose..
Melting Point 219 °C
426 °F
ASTM D3418
SK Chemicals SKYPEL P147D Productivity Grade
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti..
Melting Point <= 219 °C
<= 426 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 200.48 Low Density Polyethylene Resin
Product Description: LD 200.48 is a general purpose LDPE extrusion coating grade, designed for flexible packaging applications. It offers – Low neck-in – Very good adhesion – Excellent heat seala..
Melting Point <= 219 °C
<= 426 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 202.48 Low Density Polyethylene Resin
Product Description: LD 202.48 is an LDPE coating grade, especially designed for high speed, lightweight extrusion coating applications providing: -high speed processability – good heat sealing pro..
Melting Point <= 219 °C
<= 426 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 259 Low Density Polyethylene Resin (European Grade)
Product Description: LD 259 is a LDPE extrusion coating grade, especially introduced for coating on non-woven substrates. Its high melt-index combines with low density gives this grade the right bal..
Melting Point <= 219 °C
<= 426 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 361BW Low Density Polyethylene Resin
Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Melting Point <= 219 °C
<= 426 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 361HF Low Density Polyethylene Resin
Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Melting Point <= 219 °C
<= 426 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 361JD Low Density Polyethylene Resin
Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Melting Point <= 219 °C
<= 426 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 362BR Low Density Polyethylene Resin
Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Melting Point <= 219 °C
<= 426 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 362BW Low Density Polyethylene Resin
Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Melting Point <= 219 °C
<= 426 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 362HE Low Density Polyethylene Resin
Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Melting Point <= 219 °C
<= 426 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 362ON Low Density Polyethylene Resin
Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava..
Melting Point <= 219 °C
<= 426 °F
Peak Melting Point; ExxonMobil method
ExxonMobil LDPE LD 364HE Low Density Polyethylene Resin
Product Description: LD 364HE is an LDPE, offering a good combination of mechanical, optical and sealing properties.Availability: Africa & Middle East and Europe Additive: Antiblock: 1500 ppmSlip: ..
Melting Point 219 °C
426 °F
ASTM D3418
Ashley Polymers Ashlene® 982 Nylon 612
General purpose for extrusion. These resins are notes for their low moisture absorption and excellent dimensional stability. Bristle grade, high viscosity.Data provided by the manufacturer
Melting Point 219 °C
426 °F
ASTM D3418
Ashley Polymers Ashlene® 990L-40G Nylon 610, 40% Glass Reinforced
40% glass reinforced, excellent dimensional stability and low water absorption. Also available as: 990LS-40G, same with heat stabilizer.Data provided by the manufacturer
Melting Point 219 °C
426 °F
ASTM D789
Chem Polymer Durlex 709 IH PBT, Impact Modified
A highly impact modified PBT exhibiting excellent toughness and processability.Data provided by the manufacturer, Chem Polymer.
Melting Point 219 °C
426 °F
10°C/min; ISO 11357-1/-3
Lanxess Pocan® DP C 1502 702353 PBT+PC  (discontinued **)
PBT+PC, non-reinforced, injection molding, impact modified, low tendency to warp, UV-stabilized
Melting Point 219 °C
426 °F
DAM; ASTM D3418
DuPont Performance Polymers Zytel® FE5382 BK276 Nylon 612  (Unverified Data**)
Zytel® FE5382 BK276 is a 33% glass fiber reinforced, heat stabilized, black polyamide 612 resin developed for electrical bobbins and encapsulation applications.Information provided by DuPont Perfor..