Material Notes:
General purpose for extrusion. These resins are notes for their low moisture absorption and excellent dimensional stability. Bristle grade, high viscosity.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Water Absorption 0.37 %
0.37 %
24 hrs; ASTM D570
Water Absorption at Saturation 2.8 %
2.8 %
ASTM D570
Linear Mold Shrinkage 0.011 cm/cm
0.011 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 46.0 MPa
6670 psi
ASTM D638
Elongation at Break 250 %
250 %
ASTM D638
Flexural Modulus 2.30 GPa
334 ksi
ASTM D790
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
0.500 J/cm

@Temperature -40.0 °C
0.937 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 50.0 µm/m-°C

@Temperature 20.0 °C
27.8 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 219 °C
426 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 155 °C
311 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
140 °F
ASTM D648
Users viewing this material also viewed the following: