ExxonMobil LDPE LD 259 Low Density Polyethylene Resin (European Grade)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Exxon Chemical
Trade Name LDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LDPE LD 259 Low Density Polyethylene Resin (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LD 259 is a LDPE extrusion coating grade, especially introduced for coating on non-woven substrates. Its high melt-index combines with low density gives this grade the right balance between: -Adhesion onto non-wovens – Flexibility after coating – Barrier for fluids and gases LD 259 can also be used as a general extrusion and co-extrusion coating grade, showing – Easy processability – Good neck-in/draw down balance – Excellent heat sealability Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications: Coextrusion CoatingDemanding Heat SealsDocument PlastificationExtrusion CoatingExtrusion LaminationFood packagingHigh Speed, Thin Weight CoatingsIndustrial PackagingNon-woven coatingPhotographic PaperThermal LaminationInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.915 g/cc
0.0331 lb/in³
ExxonMobil method
Melt Flow 12 g/10 min
12 g/10 min
ASTM D1238
Neck In 4.32 cm

@Temperature 315 °C
1.70 in

@Temperature 599 °F
656 ft/min, Constant output at 35 rpm; ExxonMobil Method
4.57 cm

@Temperature 315 °C
1.80 in

@Temperature 599 °F
328 ft/min, Constant output at 35 rpm; ExxonMobil Method
Drawdown 9.17 m/s

@Temperature 315 °C
1810 ft/min

@Temperature 599 °F
Constant output at 35 rpm; ExxonMobil Method
Thermal Properties Metric English Comments
Melting Point <= 219 °C
<= 426 °F
Peak Melting Point; ExxonMobil method