Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chem Polymer Durlex 709 IH PBT, Impact Modified

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Impact Grade
Manufacturer Chem Polymer
Trade Name Durlex
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chem Polymer Durlex 709 IH PBT, Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A highly impact modified PBT exhibiting excellent toughness and processability.Data provided by the manufacturer, Chem Polymer.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Melt Flow 4.0 g/10 min
4.0 g/10 min
Condition T
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 35.0 MPa
5080 psi
ASTM D638
Elongation at Break 90 %
90 %
ASTM D638
Flexural Yield Strength 45.0 MPa
6530 psi
ASTM D790
Flexural Modulus 1.60 GPa
232 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
2.24 J/cm

@Temperature -40.0 °C
4.20 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 219 °C
426 °F
ASTM D789
Processing Properties Metric English Comments
Melt Temperature 254 °C
489 °F