Material Notes:
SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plastics to low hardness rubber. It is a kind of thermoplastic elastomer, which can be molded with general plastic mold by plasticizing at high temperature.Information provided by SK Chemicals
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Water Absorption 1.7 %
1.7 %
24 hour; ASTM D570
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
ASTM D955
Melt Flow 18 g/10 min

@Load 2.16 kg,
Temperature 230 °C
18 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 47
47
ASTM D2240
Tensile Strength, Ultimate 20.6 MPa
2990 psi
ASTM D638
Tensile Strength, Yield 3.92 MPa

@Strain 5.00 %
569 psi

@Strain 5.00 %
ASTM D638
7.35 MPa

@Strain 10.0 %
1070 psi

@Strain 10.0 %
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Flexural Modulus 0.117 GPa
16.9 ksi
ASTM D790
Resilience 54
54
ASTM D2632
Izod Impact, Notched 4.90 J/cm
9.18 ft-lb/in
ASTM D256
Tear Strength 95.0 kN/m
542 pli
ASTM D1004
Thermal Properties Metric English Comments
Melting Point 219 °C
426 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 62.0 °C
144 °F
ASTM D648
Users viewing this material also viewed the following: