Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NYCOA 1417HS PA 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Impact Grade
Manufacturer NYCOA, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NYCOA 1417HS PA 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
impact modified, heat stabilized, medium high impact strengthInformation provided by NYCOA, Inc.
Physical Properties Metric English Comments
Density 1.10 g/cc
0.0397 lb/in³
ASTM D792
Water Absorption 1.3 %
1.3 %
ASTM D570
Linear Mold Shrinkage 0.015 cm/cm
0.015 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 64.0 MPa
9280 psi
ASTM D638
Elongation at Break >= 75 %
>= 75 %
ASTM D638
Flexural Yield Strength 91.0 MPa
13200 psi
ASTM D790
Flexural Modulus 2.103 GPa
305.0 ksi
ASTM D790
Izod Impact, Notched 1.70 J/cm
3.18 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 219 °C
426 °F
ASTM D789
Processing Properties Metric English Comments
Processing Temperature 250 °C
482 °F
Rear Barrel Temperature 220 °C
428 °F
Middle Barrel Temperature 230 °C
446 °F
Front Barrel Temperature 250 °C
482 °F
Nozzle Temperature 250 °C
482 °F
Mold Temperature 80.0 °C
176 °F
Drying Temperature 76.0 °C
169 °F
Copyright © lookpolymers.com All Rights Reserved