ExxonMobil LDPE LD 364HE Low Density Polyethylene Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Exxon Chemical
Trade Name LDPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LDPE LD 364HE Low Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: LD 364HE is an LDPE, offering a good combination of mechanical, optical and sealing properties.Availability: Africa & Middle East and Europe Additive: Antiblock: 1500 ppmSlip: 550 ppmThermal Stabilizer: YesApplications: Co-Extrusion FilmsFoamsForm Fill and Seal PackagingFreezer Film High Clarity FilmLamination FilmPoultry BagRice Bags Information provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.928 g/cc
0.0335 lb/in³
ExxonMobil method
Melt Flow 0.60 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.60 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 1500 ppm
1500 ppm
Slip Level 550 ppm
550 ppm
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 320 %
320 %
ASTM D882
Film Elongation at Break, TD 560 %
560 %
ASTM D882
Elmendorf Tear Strength MD 130 g
130 g
ASTM D1922
Elmendorf Tear Strength TD 180 g
180 g
ASTM D1922
Dart Drop Test 270 g
0.595 lb
ASTM D1709A
Film Tensile Strength at Break, MD 24.1 MPa
3500 psi
ASTM D882
Film Tensile Strength at Break, TD 22.1 MPa
3200 psi
ASTM D882
1% Secant Modulus, MD 159 MPa
23000 psi
ASTM D882
1% Secant Modulus, TD 172 MPa
25000 psi
ASTM D882
Thermal Properties Metric English Comments
Melting Point <= 219 °C
<= 426 °F
Peak Melting Point; ExxonMobil method
Optical Properties Metric English Comments
Haze 6.5 %
6.5 %
ASTM D1003
Gloss 65 %
65 %
45°; ASTM D2457