Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Oxford Polymers Oxnilon 6-33GF 33% Glass Fiber Filled Nylon 6 for Injection Molding

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 30% Glass Fiber Filled
Manufacturer Oxford Polymers
Trade Name Oxnilon
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Oxford Polymers Oxnilon 6-33GF 33% Glass Fiber Filled Nylon 6 for Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
33% Glass Fiber Filled Nylon 6 for Injection MoldingInformation provided by Oxford Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Filler Content 33 %
33 %
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 172 MPa
25000 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Flexural Strength 269 MPa
39000 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 0.961 J/cm

@Temperature 23.0 °C
1.80 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 219 °C
426 °F
Deflection Temperature at 1.8 MPa (264 psi) 210 °C
410 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 271 - 288 °C
520 - 550 °F