Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 51.7 MPa
7500 psi
Mykroy/Mycalex MM 561 Molding Grade Glass-bonded Mica Composite
Synthetic mica filler. Does not burn. Good radiation resistance (3 x 10^10 Rads-Cobalt). ROHS CompliantThis ceramoplastic material is a versatile and efficient insulating material designed to meet..
Tensile Strength, Ultimate 51.7 MPa
7500 psi
ASTM D638
Nylene® Vexel™ B50U , High Flow, Un-reinforced PBT
Description: Vexel™ B50U is a high flow, un-reinforced PBT. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporatio..
Tensile Strength, Ultimate 51.7 - 241 MPa
7500 - 35000 psi
Average value: 94.5 MPa Grade Count:21
Overview of materials for Polyphthalamide (PPA), Aramid Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Aramid Fiber". Each property range of values reported is minimum and maximum values of ..
Tensile Strength, Ultimate 51.7 - 2070 MPa
7500 - 300000 psi
Average value: 207 MPa Grade Count:186
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Tensile Strength, Ultimate 51.7 MPa
7500 psi
ASTM Data
Americas Styrenics Styron® 613 Polystyrene  (discontinued **)
STYRON® 613 high heat, high strength general purpose polystyrene is typically used in applications requiring a clear, tough part such as office products and magnetic media enclosures. It offers goo..
Tensile Strength, Ultimate 51.7 MPa
7500 psi
Indium Corp. Indalloy® 106 (Sn63) Sn-Pb Solder Alloy
Standard eutectic tin-lead solder with wide application. Not recommended against silver and/or gold.Information provided by the manufacturer, Indium Corporation.
Tensile Strength, Ultimate 51.7 MPa

@Temperature 149 °C
7500 psi

@Temperature 300 °F
Greene Tweed Arlon® 1000 Polyketone
Arlon® is a tough, high-temperature, semi-crystalline, thermoplastic presenting a unique combination of mechanical, thermal, chemical and electrical properties. Greene, Tweed uses several proprie..
Tensile Strength, Ultimate 51.7 MPa
7500 psi
ASTM D638-95
Multibase Multi-ABS 7522 R , 22% Filler Content
Data provided by Multibase.
Tensile Strength, Ultimate 51.7 MPa
7500 psi
ASTM D638
Saint-Gobain Meldin® 7022 Isostatically Molded Graphite Filled Polyimide
Finished parts and basic shapes made from 40% by weight graphite filled polyimide material for applications requiring a low coefficient of thermal expansion, self lubricating properties, and good di..
Tensile Strength, Ultimate 51.7 MPa
7500 psi
Williams Advanced Alloys WS183 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Tensile Strength, Ultimate 51.7 MPa
7500 psi
ASTM D412
Lubrizol Estane® ETE 70DT3 Thermoplastic Polyurethane, Easy-to-Extrude
Type: Estane® ETE 70DT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, hig..
Tensile Strength, Ultimate 51.7 MPa
7500 psi
Crosswise; ASTM D638
Bedford Plastics Glass Reinforced FR Polyester Flat Sheet, 1/8"
Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod..
Tensile Strength, Ultimate 51.7 MPa
7500 psi
Crosswise; ASTM D638
Bedford Plastics Glass Reinforced Vinylester Flat Sheet, 1/8"
Flame retardant grade; see details in the property table.Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded prod..
Tensile Strength, Ultimate 51.7 MPa
7500 psi
Crosswise; ASTM D638
Bedford Plastics Glass Reinforced Polyester Flat Sheet 1/8"
Pultrusion results in the production and supply of one of the worlds strongest and most durable products available today. The pultruded products feature:High StrengthCorrosion Resistant to many che..
Tensile Strength, Ultimate 51.7 - 70.0 MPa
7500 - 10200 psi
Average value: 61.7 MPa Grade Count:6
Overview of materials for PC/ABS + Stainless Steel
This property data is a summary of similar materials in the MatWeb database for the category "PC/ABS + Stainless Steel". Each property range of values reported is minimum and maximum values of appro..
Tensile Strength, Ultimate 51.7 - 124 MPa
7500 - 18000 psi
Average value: 81.9 MPa Grade Count:11
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Glass Fiber Filler". Each property range of values reported is minimum and ..
Tensile Strength, Ultimate 51.7 MPa
7500 psi
TM R050-36
Resinlab® EP1026 Clear Epoxy Adhesive
Resinlab™ EP1026 Clear is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in ..
Tensile Strength, Ultimate 51.7 MPa
7500 psi
TM R050-36
Resinlab® EP11HT Gray Filled Epoxy Adhesive
Resinlab™ EP11HT Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa..
Tensile Strength, Ultimate 51.7 MPa
7500 psi
TM R050-36
Resinlab® EP965SC-7 Black Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP965SC-7 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wett..
Tensile Strength, Ultimate 51.7 MPa
7500 psi
TM R050-36
Resinlab® EP965SC-7 Clear Unfilled Electronic Grade Epoxy Encapsulant
Resinlab™ EP965SC-7 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wett..
Tensile Strength, Ultimate 51.7 MPa
7500 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Edgetek® UR-30GF/000 Thermoplastic Elastomer - TPU, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Strength, Ultimate 51.7 MPa
7500 psi
Film; ASTM D412
AdvanSource Biomaterials ChronoFlex® AR Biodurable Medical Grade Polyurethane
AdvanSource Biomaterials Corporation manufactures and markets this solution-grade, segmented, aromatic, polycarbonate-based polyurethane designed for use in solvent casting and dipping applications...
Tensile Strength, Ultimate 51.7 MPa
7500 psi
TM R050-36
Resinlab® EP1026 Black Epoxy Adhesive
Resinlab™ EP1026 Black is a two part unfilled epoxy adhesive designed for high speed bonding of metals, ceramics, and most plastics. It cures to a tough semi-rigid material, and is free flowing in ..
Tensile Strength, Ultimate 51.7 - 72.4 MPa
7500 - 10500 psi
ASTM D638
Premix Premi-Glas® 1200H-24 Polyester SMC  (discontinued **)
Premi-Glas® 1200H-24 is a 24% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where arc resistance and dielectric strength are required and UL 94 HB flame recogni..