Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "PC/ABS + Stainless Steel". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.19 - 1.52 g/cc
0.0430 - 0.0549 lb/in³
Average value: 1.31 g/cc Grade Count:8
Filler Content 5.00 - 20.0 %
5.00 - 20.0 %
Average value: 9.40 % Grade Count:5
Water Absorption 0.100 - 0.120 %
0.100 - 0.120 %
Average value: 0.107 % Grade Count:6
Linear Mold Shrinkage 0.00100 - 0.0100 cm/cm
0.00100 - 0.0100 in/in
Average value: 0.00525 cm/cm Grade Count:7
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 51.7 - 70.0 MPa
7500 - 10200 psi
Average value: 61.7 MPa Grade Count:6
Elongation at Break 2.00 - 10.0 %
2.00 - 10.0 %
Average value: 4.96 % Grade Count:7
Modulus of Elasticity 2.69 - 5.50 GPa
390 - 798 ksi
Average value: 3.34 GPa Grade Count:6
Flexural Yield Strength 82.7 - 134 MPa
12000 - 19500 psi
Average value: 102 MPa Grade Count:7
Flexural Modulus 2.34 - 3.79 GPa
340 - 550 ksi
Average value: 3.04 GPa Grade Count:7
Izod Impact, Notched 0.427 - 5.87 J/cm
0.800 - 11.0 ft-lb/in
Average value: 1.43 J/cm Grade Count:7
Izod Impact, Unnotched 2.14 - 10.7 J/cm
4.00 - 20.0 ft-lb/in
Average value: 6.83 J/cm Grade Count:5
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 113 - 130 °C
235 - 266 °F
Average value: 120 °C Grade Count:3
Deflection Temperature at 1.8 MPa (264 psi) 104 - 120 °C
220 - 248 °F
Average value: 112 °C Grade Count:6
Flammability, UL94 HB - V-0
HB - V-0
Grade Count:5
Electrical Properties Metric English Comments
Electrical Resistivity 1.00 - 10000 ohm-cm
1.00 - 10000 ohm-cm
Average value: 1690 ohm-cm Grade Count:7
Surface Resistance 1.00 - 1.00e+6 ohm
1.00 - 1.00e+6 ohm
Average value: 573000 ohm Grade Count:7
Static Decay 0.100 - 2.00 sec
0.100 - 2.00 sec
Average value: 1.68 sec Grade Count:6
Processing Properties Metric English Comments
Processing Temperature 232 - 266 °C
450 - 510 °F
Average value: 249 °C Grade Count:5
Mold Temperature 50.0 - 93.3 °C
122 - 200 °F
Average value: 70.4 °C Grade Count:6
Injection Pressure 68.9 - 103 MPa
10000 - 15000 psi
Average value: 86.2 MPa Grade Count:5