Polymer Property : Compressive Strength = 55.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 55.0 MPa

@Temperature 200 °C
7980 psi

@Temperature 392 °F
ISO 604
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c..
Compressive Strength 55.0 MPa

@Temperature 200 °C
7980 psi

@Temperature 392 °F
ISO 604
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F..
Compressive Strength 55.0 MPa

@Temperature 200 °C
7980 psi

@Temperature 392 °F
Result based on 450GL30; ISO 604
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black
Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos..
Compressive Strength 55.0 MPa

@Temperature 200 °C
7980 psi

@Temperature 392 °F
ISO 604
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, ..
Compressive Strength 55.0 MPa

@Temperature 250 °C
7980 psi

@Temperature 482 °F
ISO 604
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta..
Compressive Strength 55.0 MPa

@Temperature 250 °C
7980 psi

@Temperature 482 °F
ISO 604
Victrex® WG102™ Polyaryletherketone
Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c..
Compressive Strength 55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 150 AC Dense Refractory Castable
Description: Curon 150 AC is a coarse castable for use up to 1500°C with a high strength.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Compressive Strength 55.0 - 65.0 MPa

@Temperature 1300 °C
7980 - 9430 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast CURON 150 HS Dense Refractory Castable
Description: Dense refractory castableRemarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast.
Compressive Strength 55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 160 FS Dense Refractory Castable
Description: This castable is based on fused silica. It has an extremely good thermal shock resistance and minor expansion behavior up to process temperature of 900°C. Application: zinc melting f..
Compressive Strength 55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 160 HC Dense Refractory Castable
Description: Because of the selection of raw materials, this castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HC has an excellent thermal s..
Compressive Strength 55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 160 HS GM Dense Refractory Castable
Description: This gunning castable has a high volume stability up to high temperatures. In addition Curon 160 HS GM has an excellent thermal shock resistance and abrasion resistance (9-12 cm3 accord..
Compressive Strength 55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 180 B Dense Refractory Castable
Description: This high quality castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of Fe2O3, this castable can..
Compressive Strength 55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 180 Dense Refractory Castable
Description: This high quality, corundum based castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of SiO2, th..
Compressive Strength 55.0 - 65.0 MPa

@Temperature 110 °C
7980 - 9430 psi

@Temperature 230 °F
Cold Crushing Strength
Gouda Vuurvast FLUCON 150 G (R) Dense Self Flowing Refractory Castable
Description: Flucon 150 G (R) is a self-flowing low cement castable based on sintered South-American bauxite. Especially suitable for direct contact with liquid aluminum metal.Remarks: These values ..
Compressive Strength 55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 135 Dense Vibrating Refractory Castable
Description: Vibron 135 is a vibrating castable, specially fit for the production of prefab elements. The very low cement content (1%) and the abrasion resistant spinel grains give this material exc..
Compressive Strength 55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 140 C RAPID Dense Vibrating Refractory Castable
Description: Vibron 140 C Rapid is a low cement castable, based on high quality coarse chamotte grog. Because of special additives this castable is special suited for a faster heating schedule.Remar..
Compressive Strength 55.0 - 65.0 MPa

@Temperature 1300 °C
7980 - 9430 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast CURON 14 S Dense Refractory Castable
Description: Curon 14 S is a dense, strong and abrasion resistant castable. Because of the very low percentage of Fe2O3 and SiO2 it is used for highly abrasive conditions in reducing atmospheres.Rem..
Compressive Strength 55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 160 H Dense Refractory Castable
Description: Because of the selection of raw materials this castable has a high volume stability and keeps its strength up to high temperatures. In addition Curon 160 H has an excellent thermal shoc..
Compressive Strength 55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 155 Dense Vibrating Refractory Castable
Description: Vibron 155 is a vibrating castable based on sintered bauxite especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provid..
Compressive Strength 55.0 MPa

@Strain 1 %
7980 psi

@Strain 1 %
ISO 604
Quadrant EPP Duratron® PAI T5530 PAI, 30% glass fibers, compression moulded (ISO Data)
This 30 % glass fibre reinforced grade offers higher stiffness, strength and creep resistance than the Duratron PAI grades mentioned above. It is well suited for structural applications supporting s..
Compressive Strength 55.0 MPa

@Temperature 200 °C
7980 psi

@Temperature 392 °F
ISO 604
Victrex® PEEK 150GL30 Black Polyetheretherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact co..