Gouda Vuurvast FLUCON 150 G (R) Dense Self Flowing Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Gouda Vuurvast
Trade Name FLUCON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast FLUCON 150 G (R) Dense Self Flowing Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Flucon 150 G (R) is a self-flowing low cement castable based on sintered South-American bauxite. Especially suitable for direct contact with liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.75 - 2.85 g/cc
0.0994 - 0.103 lb/in³
After drying at 110°C
Particle Size <= 5000 µm
<= 5000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 55.0 - 65.0 MPa

@Temperature 110 °C
7980 - 9430 psi

@Temperature 230 °F
Cold Crushing Strength
170 - 190 MPa

@Temperature 1200 °C
24700 - 27600 psi

@Temperature 2190 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.40 - 1.60 W/m-K

@Temperature 1200 °C
9.72 - 11.1 BTU-in/hr-ft²-°F

@Temperature 2190 °F
1.60 - 1.80 W/m-K

@Temperature 110 °C
11.1 - 12.5 BTU-in/hr-ft²-°F

@Temperature 230 °F
Maximum Service Temperature, Air 1350 °C
2460 °F
Shrinkage -0.100 - 0.200 %

@Temperature 1200 °C
-0.100 - 0.200 %

@Temperature 2190 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 78 %
78 %
Fe2O3 <= 1.0 %
<= 1.0 %
SiO2 12 %
12 %
Descriptive Properties Value Comments
Material Consumption per 1 m3 2750 kg
Mixing Water 6-7 liters
per 100 kgs dry material