Material Notes:
Description: This castable is based on fused silica. It has an extremely good thermal shock resistance and minor expansion behavior up to process temperature of 900°C. Application: zinc melting furnace inductors.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.00 - 2.10 g/cc
0.0723 - 0.0759 lb/in³
After drying at 110°C
Particle Size <= 5000 µm
<= 5000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 35.0 - 45.0 MPa

@Temperature 1000 °C
5080 - 6530 psi

@Temperature 1830 °F
Cold Crushing Strength
55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.10 - 1.20 W/m-K

@Temperature 100 °C
7.63 - 8.33 BTU-in/hr-ft²-°F

@Temperature 212 °F
1.13 - 1.23 W/m-K

@Temperature 600 °C
7.84 - 8.54 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.16 - 1.26 W/m-K

@Temperature 1000 °C
8.05 - 8.74 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Maximum Service Temperature, Air 1600 °C
2910 °F
Shrinkage -0.100 - 0.100 %

@Temperature 1000 °C
-0.100 - 0.100 %

@Temperature 1830 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 20 %
20 %
Fe2O3 0.10 %
0.10 %
SiO2 75 %
75 %
Descriptive Properties Value Comments
ASTM Classification E
Material Consumption per 1 m3 1950 kg
Mixing Water 8-10 liters
per 100 kgs dry material