Gouda Vuurvast CURON 180 B Dense Refractory Castable

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer Gouda Vuurvast
Trade Name CURON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Gouda Vuurvast CURON 180 B Dense Refractory Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: This high quality castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of Fe2O3, this castable can be applied in reducing atmospheres.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.65 - 2.75 g/cc
0.0957 - 0.0994 lb/in³
After drying at 110°C
Particle Size <= 6000 µm
<= 6000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 40.0 - 50.0 MPa

@Temperature 1600 °C
5800 - 7250 psi

@Temperature 2910 °F
Cold Crushing Strength
55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 1.28 - 1.48 W/m-K

@Temperature 600 °C
8.88 - 10.3 BTU-in/hr-ft²-°F

@Temperature 1110 °F
1.35 - 1.55 W/m-K

@Temperature 1600 °C
9.37 - 10.8 BTU-in/hr-ft²-°F

@Temperature 2910 °F
1.45 - 1.65 W/m-K

@Temperature 100 °C
10.1 - 11.5 BTU-in/hr-ft²-°F

@Temperature 212 °F
Maximum Service Temperature, Air 1800 °C
3270 °F
Shrinkage -0.250 - 0.250 %

@Temperature 1600 °C
-0.250 - 0.250 %

@Temperature 2910 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 90 %
90 %
CaO 4.0 %
4.0 %
Fe2O3 1.0 %
1.0 %
SiO2 4.0 %
4.0 %
Descriptive Properties Value Comments
ASTM Classification G
Material Consumption per 1 m3 2650 kg
Mixing Water 8-10 liters
per 100 kgs dry material