Material Notes:
Description: Because of the selection of raw materials, this castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HC has an excellent thermal shock resistance. It is largely used in the steel industry.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.30 - 2.40 g/cc
0.0831 - 0.0867 lb/in³
After drying at 110°C
Particle Size <= 8000 µm
<= 8000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 40.0 - 50.0 MPa

@Temperature 1000 °C
5800 - 7250 psi

@Temperature 1830 °F
Cold Crushing Strength
55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.550 - 0.650 W/m-K

@Temperature 100 °C
3.82 - 4.51 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.670 - 0.770 W/m-K

@Temperature 600 °C
4.65 - 5.34 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.740 - 0.840 W/m-K

@Temperature 1000 °C
5.14 - 5.83 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Maximum Service Temperature, Air 1600 °C
2910 °F
Shrinkage -0.200 - 0.200 %

@Temperature 1000 °C
-0.200 - 0.200 %

@Temperature 1830 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 61 %
61 %
Fe2O3 <= 1.5 %
<= 1.5 %
SiO2 30 %
30 %
Descriptive Properties Value Comments
ASTM Classification E
Material Consumption per 1 m3 2300 kg
Mixing Water 8-10 liters
per 100 kgs dry material