Mechanical Properties Metric English Comments
Compressive Strength 55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 150 AC Dense Refractory Castable
Description: Curon 150 AC is a coarse castable for use up to 1500°C with a high strength.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Compressive Strength 55.0 - 65.0 MPa

@Temperature 1300 °C
7980 - 9430 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast CURON 150 HS Dense Refractory Castable
Description: Dense refractory castableRemarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast.
Compressive Strength 55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 160 FS Dense Refractory Castable
Description: This castable is based on fused silica. It has an extremely good thermal shock resistance and minor expansion behavior up to process temperature of 900°C. Application: zinc melting f..
Compressive Strength 55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 160 HC Dense Refractory Castable
Description: Because of the selection of raw materials, this castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HC has an excellent thermal s..
Compressive Strength 55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 160 HS GM Dense Refractory Castable
Description: This gunning castable has a high volume stability up to high temperatures. In addition Curon 160 HS GM has an excellent thermal shock resistance and abrasion resistance (9-12 cm3 accord..
Compressive Strength 55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 180 B Dense Refractory Castable
Description: This high quality castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of Fe2O3, this castable can..
Compressive Strength 55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 180 Dense Refractory Castable
Description: This high quality, corundum based castable is marked by a high refractoriness and a good thermal shock resistance. Because it has a high alumina content and a low percentage of SiO2, th..
Compressive Strength 55.0 - 65.0 MPa

@Temperature 110 °C
7980 - 9430 psi

@Temperature 230 °F
Cold Crushing Strength
Gouda Vuurvast FLUCON 150 G (R) Dense Self Flowing Refractory Castable
Description: Flucon 150 G (R) is a self-flowing low cement castable based on sintered South-American bauxite. Especially suitable for direct contact with liquid aluminum metal.Remarks: These values ..
Compressive Strength 55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 135 Dense Vibrating Refractory Castable
Description: Vibron 135 is a vibrating castable, specially fit for the production of prefab elements. The very low cement content (1%) and the abrasion resistant spinel grains give this material exc..
Compressive Strength 55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 140 C RAPID Dense Vibrating Refractory Castable
Description: Vibron 140 C Rapid is a low cement castable, based on high quality coarse chamotte grog. Because of special additives this castable is special suited for a faster heating schedule.Remar..
Compressive Strength 55.0 - 65.0 MPa

@Temperature 1300 °C
7980 - 9430 psi

@Temperature 2370 °F
Cold Crushing Strength
Gouda Vuurvast CURON 14 S Dense Refractory Castable
Description: Curon 14 S is a dense, strong and abrasion resistant castable. Because of the very low percentage of Fe2O3 and SiO2 it is used for highly abrasive conditions in reducing atmospheres.Rem..
Compressive Strength 55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast CURON 160 H Dense Refractory Castable
Description: Because of the selection of raw materials this castable has a high volume stability and keeps its strength up to high temperatures. In addition Curon 160 H has an excellent thermal shoc..
Compressive Strength 55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Gouda Vuurvast VIBRON 155 Dense Vibrating Refractory Castable
Description: Vibron 155 is a vibrating castable based on sintered bauxite especially fit for the production of prefab elements.Remarks: Indicated values apply to vibrated products.Information provid..