Quadrant EPP Duratron® PAI T5530 PAI, 30% glass fibers, compression moulded (ISO Data)

Category Polymer , Thermoplastic , Polyamide-imide (PAI) , Polyamide-Imide, Glass Filled
Manufacturer Quadrant Engineering Plastics Products
Trade Name Duratron® PAI
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quadrant EPP Duratron® PAI T5530 PAI, 30% glass fibers, compression moulded (ISO Data).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This 30 % glass fibre reinforced grade offers higher stiffness, strength and creep resistance than the Duratron PAI grades mentioned above. It is well suited for structural applications supporting static loads for long periods of time at high temperatures. In addition, Duratron T5530 PAI exhibits superb dimensional stability up to 250 °C making it extremely popular for precision parts in e.g. the electronical and semiconductor industries. The suitability of Duratron T5530 PAI for sliding parts, however, is to be carefully examined since the glass fibres tend to abrade the mating surface. Very high maximum allowable service temperature in air (250°C continuously) Excellent retention of mechanical strength, stiffness and creep resistance over a wide temperature range Dimensional stability up to 260°C Excellent wear & frictional behaviour (particulary Duratron T4301 & T4501 PAI) Very good UV-resistanceGood resistance against high energy radiation (gamma- and X-rays) Inherent low flammability
Physical Properties Metric English Comments
Density 1.61 g/cc
0.0582 lb/in³
ISO 1183-1
Moisture Absorption at Equilibrium 1.7 %
1.7 %
50% RH
Water Absorption at Saturation 3.2 %
3.2 %
Mechanical Properties Metric English Comments
Hardness, Rockwell E 85
85
ISO 2039-2
Hardness, Shore D 90
90
Ball Indentation Hardness 275 MPa
39900 psi
ISO 2039-1
Tensile Strength 125 MPa
18100 psi
at Break (NYP); ISO 527-1/-2
Elongation at Break 3.0 %
3.0 %
ISO 527-1/-2
Tensile Modulus 6.40 GPa
928 ksi
ISO 527-1/-2
Flexural Strength 170 MPa
24700 psi
Compressive Strength 55.0 MPa

@Strain 1 %
7980 psi

@Strain 1 %
ISO 604
104 MPa

@Strain 2 %
15100 psi

@Strain 2 %
ISO 604
190 MPa

@Strain 5 %
27600 psi

@Strain 5 %
ISO 604
Charpy Impact Unnotched 3.00 J/cm²
14.3 ft-lb/in²
ISO 179-1/1eU
Charpy Impact, Notched 0.350 J/cm²
1.67 ft-lb/in²
ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.35 - 0.60
0.35 - 0.60
Thermal Properties Metric English Comments
CTE, linear 35.0 µm/m-°C

@Temperature 23.0 - 100 °C
19.4 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.360 W/m-K
2.50 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 250 °C
482 °F
Continuous
Deflection Temperature at 1.8 MPa (264 psi) 280 °C
536 °F
ISO 75-1/-2
Glass Transition Temp, Tg 280 °C
536 °F
DSC, 20°C/min.; ISO 11357-1/-2
Flammability, UL94 V-0
V-0
Oxygen Index 50 %
50 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity >= 1.0e+14 ohm-cm
>= 1.0e+14 ohm-cm
IEC 60093
Surface Resistivity per Square >= 1.0e+13 ohm
>= 1.0e+13 ohm
IEC 60093
Dielectric Constant 4.4

@Frequency >=100000 Hz
4.4

@Frequency >=100000 Hz
IEC 60250
Dielectric Strength 28.0 kV/mm
711 kV/in
Dissipation Factor 0.022

@Frequency 100000 Hz
0.022

@Frequency 100000 Hz
IEC 60250
Comparative Tracking Index 175 V
175 V
IEC 60112
Compliance Properties Metric English Comments
3A-Dairy No
No
European Food 1935/2004 No
No
FDA No
No
USP Class VI No
No
Chemical Resistance Properties Metric English Comments
Acids, Strong (pH 1-3) Limited
Limited
Acids, Weak Acceptable
Acceptable
Alcohols Acceptable
Acceptable
Alkalies, Strong (pH 11-14) Unacceptable
Unacceptable
Alkalies, Weak Limited
Limited
Chlorinated Solvents Acceptable
Acceptable
Continuous Sunlight Limited
Limited
Hot Water / Steam Limited
Limited
Hydrocarbons - Aliphatic Acceptable
Acceptable
Hydrocarbons - Aromatic Acceptable
Acceptable
Inorganic Salt Solutions Acceptable
Acceptable
Ketones, Esters Acceptable
Acceptable