Material Notes:
Description: This gunning castable has a high volume stability up to high temperatures. In addition Curon 160 HS GM has an excellent thermal shock resistance and abrasion resistance (9-12 cm3 according to ASTM C704-76a).Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 2.25 - 2.35 g/cc
0.0813 - 0.0849 lb/in³
After drying at 110°C
Particle Size <= 6000 µm
<= 6000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 45.0 - 55.0 MPa

@Temperature 1400 °C
6530 - 7980 psi

@Temperature 2550 °F
Cold Crushing Strength
55.0 - 65.0 MPa

@Temperature 100 °C
7980 - 9430 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.590 - 0.690 W/m-K

@Temperature 100 °C
4.09 - 4.79 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.650 - 0.750 W/m-K

@Temperature 600 °C
4.51 - 5.20 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.820 - 0.920 W/m-K

@Temperature 1400 °C
5.69 - 6.38 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Maximum Service Temperature, Air 1600 °C
2910 °F
Shrinkage -0.400 - 0.400 %

@Temperature 1400 °C
-0.400 - 0.400 %

@Temperature 2550 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 65 %
65 %
CaO 4.0 %
4.0 %
Fe2O3 <= 1.5 %
<= 1.5 %
SiO2 29 %
29 %
Descriptive Properties Value Comments
ASTM Classification E
Material Consumption per 1 m3 2250 kg