BASF Procom® D 1133 Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer BASF
Trade Name Procom®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Procom® D 1133 Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data was collected by ISO methods and provided by BASF.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Linear Mold Shrinkage, Flow 0.011 cm/cm
0.011 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 26.0 MPa
3770 psi
Elongation at Break 11 %
11 %
Tensile Modulus 2.40 GPa
348 ksi
Charpy Impact Unnotched 5.00 J/cm²
23.8 ft-lb/in²
1.50 J/cm²

@Temperature -30.0 °C
7.14 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
Vicat Softening Point 80.0 °C
176 °F