Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.50 - 8.50 J/cm² | 7.14 - 40.5 ft-lb/in² | Average value: 4.01 J/cm² Grade Count:22 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber". Each property range of values reported is minimum and maximum values of .. |
|||
Charpy Impact Unnotched | 2.10 - 8.50 J/cm² @Temperature -40.0 - -20.0 °C |
9.99 - 40.5 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 4.82 J/cm² Grade Count:4 |
Overview of materials for Nylon 66, 30% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in.. |
|||
Charpy Impact Unnotched | 1.80 - 8.50 J/cm² | 8.57 - 40.5 ft-lb/in² | Average value: 4.46 J/cm² Grade Count:77 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |