Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

EMS-Grivory Grivory® BGM-65 X V0 PA6-(GF+MD)65

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Glass/Mineral Reinforced
Manufacturer EMS-Grivory (EMS-CHEMIE)
Trade Name Grivory®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Grivory Grivory® BGM-65 X V0 PA6-(GF+MD)65.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product description: Grilon BGM-65 X V0 is a flame retardant mineral and glass fiber reinforced PA6 injection molding grade. Grilon BGM-65 X V0 has the following important properties: Halogen and phosphorous-freeLow smoke densityUL94 V-0 at 1.5 mm wall thicknessExceptional high oxygen indexHigh stiffness Grilon BGM-65 X V0 is typically used for electrical applications such as switches, plugs, lamp parts, coil former bobbins, and protective housings.Information provided by EMS Grivory
Physical Properties Metric English Comments
Density 1.69 g/cc
0.0611 lb/in³
ISO 1183
Water Absorption 5.0 %
5.0 %
ISO 62
Moisture Absorption 1.50 %
1.50 %
ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
ISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
ISO 294-4, 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 90.0 MPa
13100 psi
conditioned; ISO 527-1/-2
120 MPa
17400 psi
dry; ISO 527-1/-2
Elongation at Break 1.0 %
1.0 %
dry; ISO 527-1/-2
3.0 %
3.0 %
conditioned; ISO 527-1/-2
Tensile Modulus 7.10 GPa
1030 ksi
conditioned; ISO 527-1/-2
11.5 GPa
1670 ksi
dry; ISO 527-1/-2
Charpy Impact Unnotched 2.50 J/cm²
11.9 ft-lb/in²
dry; ISO 179/1eU
2.50 J/cm²
11.9 ft-lb/in²
conditioned; ISO 179/1eU
1.50 J/cm²

@Temperature 30.0 °C
7.14 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
1.50 J/cm²

@Temperature 30.0 °C
7.14 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
dry; ISO 179/1eA
0.300 J/cm²
1.43 ft-lb/in²
conditioned; ISO 179/1eA
0.300 J/cm²

@Temperature 30.0 °C
1.43 ft-lb/in²

@Temperature 86.0 °F
dry; ISO 179/1eU
0.300 J/cm²

@Temperature 30.0 °C
1.43 ft-lb/in²

@Temperature 86.0 °F
conditioned; ISO 179/1eU
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
16.7 µin/in-°F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
33.3 µin/in-°F
ISO 11359-1/-2
Melting Point 222 °C
432 °F
10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 110 °C
176 - 230 °F
long term; EMS
160 °C
320 °F
short term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ISO 75-1/-2
Flammability, UL94 V-0
V-0
IEC 60695-11-10
V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
IEC 60695-11-10
Oxygen Index 65 %
65 %
ISO 4589-1/-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
conditioned; IEC 60093
1.00e+14 ohm-cm
1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
IEC 60093
Dielectric Constant 3.0

@Frequency 100 Hz
3.0

@Frequency 100 Hz
dry; IEC 60250
3.0

@Frequency 100 Hz
3.0

@Frequency 100 Hz
conditioned; IEC 60250
Dielectric Strength 29.0 kV/mm
737 kV/in
conditioned; IEC 60243-1
33.0 kV/mm
838 kV/in
dry; IEC 60243-1
Comparative Tracking Index 500 V
500 V
conditioned; IEC 60112
Descriptive Properties Value Comments
Automotive Automotive electr. and electronics, lighting
Electricals & Electronics Connectors
Electrical appliances
Electrical equipment
Energy distribution
Lighting
Form Granules
Processing Injection Molding
Special Characteristics Flame retardant
Users viewing this material also viewed the following: