Mechanical Properties Metric English Comments
Charpy Impact Unnotched 0.450 - 10.0 J/cm²
2.14 - 47.6 ft-lb/in²
Average value: 4.31 J/cm² Grade Count:101
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..
Charpy Impact Unnotched 2.50 - 10.0 J/cm²
11.9 - 47.6 ft-lb/in²
Average value: 5.53 J/cm² Grade Count:4
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an..
Charpy Impact Unnotched 1.50 - 10.0 J/cm²
7.14 - 47.6 ft-lb/in²
Average value: 5.14 J/cm² Grade Count:58
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
Charpy Impact Unnotched 9.17 - 10.0 J/cm²

@Temperature -30.0 - -30.0 °C
43.6 - 47.6 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 9.59 J/cm² Grade Count:2
Overview of materials for Nylon 11 with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are includ..
Charpy Impact Unnotched 4.50 - 10.0 J/cm²
21.4 - 47.6 ft-lb/in²
Average value: 7.98 J/cm² Grade Count:20
Overview of materials for Nylon 12, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
Charpy Impact Unnotched 4.00 - 10.0 J/cm²

@Temperature -30.0 - 30.0 °C
19.0 - 47.6 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 7.89 J/cm² Grade Count:18
Overview of materials for Nylon 12, 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. ..
Charpy Impact Unnotched 6.00 - 10.0 J/cm²
28.6 - 47.6 ft-lb/in²
Average value: 8.00 J/cm² Grade Count:21
Overview of materials for Nylon 12, 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. ..
Charpy Impact Unnotched 4.00 - 10.0 J/cm²

@Temperature -30.0 - -30.0 °C
19.0 - 47.6 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 6.87 J/cm² Grade Count:42
Overview of materials for Nylon 46, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values ..
Charpy Impact Unnotched 5.00 - 10.0 J/cm²
23.8 - 47.6 ft-lb/in²
Average value: 7.06 J/cm² Grade Count:8
Overview of materials for Polystyrene, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a..