Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LATI Latimass 82-02 D030 PA12

Category Polymer , Thermoplastic , Nylon , Nylon 12
Manufacturer LATI
Trade Name Latimass
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LATI Latimass 82-02 D030 PA12.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Physical Properties Metric English Comments
Density 3.30 g/cc
0.119 lb/in³
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm
0.0080 - 0.010 in/in
Linear Mold Shrinkage, Transverse 0.0080 - 0.010 cm/cm
0.0080 - 0.010 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 25.0 MPa
3630 psi
Elongation at Break 0.60 %
0.60 %
Tensile Modulus 10.0 GPa
1450 ksi
Charpy Impact Unnotched 1.50 J/cm²
7.14 ft-lb/in²
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
302 °F
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
Vicat Softening Point 165 °C

@Load 5.00 kg
329 °F

@Load 11.0 lb
Processing Properties Metric English Comments
Melt Temperature 240 - 260 °C
464 - 500 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 - 100 °C

@Time 10800 sec
176 - 212 °F

@Time 3.00 hour
Descriptive Properties Value Comments
ISO Shrinkage - Pressure 60 MPa
Users viewing this material also viewed the following: