Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 1.00 - 2.00 J/cm² | 4.76 - 9.52 ft-lb/in² | ISO 11542-2 |
Okulen® 500 - REG PE Colored OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Charpy Impact Unnotched | 1.00 - 2.00 J/cm² | 4.76 - 9.52 ft-lb/in² | ISO 11542-2 |
Okulen® 500 PE-HMW, AST OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Charpy Impact Unnotched | 1.00 - 2.00 J/cm² | 4.76 - 9.52 ft-lb/in² | ISO 11542-2 |
Okulen® 500 PE-HMW, Coloured OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Charpy Impact Unnotched | 1.00 - 2.00 J/cm² | 4.76 - 9.52 ft-lb/in² | ISO 11542-2 |
Okulen® 500 PE-HMW, UV - stabilized OKULEN® 500 is a high molecular low pressure polyethylene with a molecular weight of approximately 500 g/mol. Applications include the food industyr and sports center construction. It does an excel.. |
|||
Charpy Impact Unnotched | 0.800 - 2.00 J/cm² | 3.81 - 9.52 ft-lb/in² | Average value: 1.53 J/cm² Grade Count:3 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Charpy Impact Unnotched | 1.50 - 2.00 J/cm² @Temperature -40.0 - -20.0 °C |
7.14 - 9.52 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 1.77 J/cm² Grade Count:2 |
Overview of materials for Polystyrene, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Charpy Impact Unnotched | 1.40 - 2.00 J/cm² @Temperature -40.0 - -20.0 °C |
6.66 - 9.52 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 1.85 J/cm² Grade Count:4 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |
|||
Charpy Impact Unnotched | 1.70 - 2.00 J/cm² | 8.09 - 9.52 ft-lb/in² | Average value: 1.83 J/cm² Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Charpy Impact Unnotched | 1.00 - 2.00 J/cm² | 4.76 - 9.52 ft-lb/in² | Average value: 1.50 J/cm² Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with PTFE Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with PTFE Filler". Each property range of values reported is minimum and max.. |
|||
Charpy Impact Unnotched | 1.90 - 2.00 J/cm² | 9.04 - 9.52 ft-lb/in² | Average value: 1.97 J/cm² Grade Count:3 |
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu.. |