Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shinkong Synthetic Fibers Shinite® PP4220 PP, High Impact, Fire Retardant

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shinkong Synthetic Fibers Shinite® PP4220 PP, High Impact, Fire Retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information from Shinkong Synthetic Fibers Corp.
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc
0.940 g/cc
ASTM D792
Water Absorption 0.050 %
0.050 %
ASTM D570
Linear Mold Shrinkage, Flow 0.014 - 0.016 cm/cm
0.014 - 0.016 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.014 - 0.016 cm/cm
0.014 - 0.016 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 26.5 MPa
3840 psi
ASTM D638
Elongation at Break 20 %
20 %
ASTM D638
Flexural Yield Strength 28.4 MPa
4120 psi
ASTM D790
Flexural Modulus 0.981 GPa
142 ksi
ASTM D790
Izod Impact, Notched 0.981 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.84 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 115 °C
239 °F
ASTM D648
Flammability, UL94 V-2
V-2