Lucent Polymers 66-01 Nylon 66, General Purpose, Injection Grade

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Lucent Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucent Polymers 66-01 Nylon 66, General Purpose, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Add "R" for Added ReleaseAdd "HU" for WeatherableTypical Properties, Dry as MoldedInformation provided by Lucent Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.014 cm/cm

@Thickness 3.17 mm
0.014 in/in

@Thickness 0.125 in
1/8" Section
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.86 MPa
11000 psi
ASTM D638
Elongation at Break >= 20 %
>= 20 %
ASTM D638
Flexural Strength 110.34 MPa
16003 psi
ASTM D790
Flexural Modulus 2.828 GPa
410.1 ksi
ASTM D790
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
0.800 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 250 - 265 °C
482 - 509 °F
ASTM D789
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ASTM D648