Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00100 - 0.0130 cm/cm | 0.00100 - 0.0130 in/in | Average value: 0.00343 cm/cm Grade Count:26 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.0130 cm/cm | 0.00200 - 0.0130 in/in | Average value: 0.00513 cm/cm Grade Count:5 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled". Each property range of values reported i.. |
|||
Linear Mold Shrinkage | 0.000600 - 0.0130 cm/cm | 0.000600 - 0.0130 in/in | Average value: 0.00759 cm/cm Grade Count:23 |
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va.. |
|||
Linear Mold Shrinkage | 0.0000900 - 0.0130 cm/cm | 0.0000900 - 0.0130 in/in | Average value: 0.00459 cm/cm Grade Count:164 |
Overview of materials for Polysulfone (PSU) This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.0130 cm/cm | 0.00100 - 0.0130 in/in | Average value: 0.00408 cm/cm Grade Count:26 |
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum .. |
|||
Linear Mold Shrinkage | 0.000500 - 0.0130 cm/cm | 0.000500 - 0.0130 in/in | Average value: 0.00447 cm/cm Grade Count:37 |
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% .. |
|||
Linear Mold Shrinkage | -0.000500 - 0.0130 cm/cm | -0.000500 - 0.0130 in/in | Average value: 0.00732 cm/cm Grade Count:22 |
Overview of materials for Melamine-Phenolic Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap.. |
|||
Linear Mold Shrinkage | 0.0100 - 0.0130 cm/cm @Temperature 150 - 150 °C |
0.0100 - 0.0130 in/in @Temperature 302 - 302 °F |
Average value: 0.0109 cm/cm Grade Count:17 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |
|||
Linear Mold Shrinkage | 0.0100 - 0.0130 cm/cm @Time 900 - 900 sec |
0.0100 - 0.0130 in/in @Time 0.250 - 0.250 hour |
Average value: 0.0109 cm/cm Grade Count:17 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.0130 cm/cm | 0.00400 - 0.0130 in/in | Average value: 0.00840 cm/cm Grade Count:25 |
Overview of materials for Polypropylene with 30% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Mica Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.0130 cm/cm | 0.00400 - 0.0130 in/in | Average value: 0.00719 cm/cm Grade Count:24 |
Overview of materials for Polypropylene with 40% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are.. |