Polymer Property : Linear Mold Shrinkage = 0.0130 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00100 - 0.0130 cm/cm
0.00100 - 0.0130 in/in
Average value: 0.00343 cm/cm Grade Count:26
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35..
Linear Mold Shrinkage 0.00200 - 0.0130 cm/cm
0.00200 - 0.0130 in/in
Average value: 0.00513 cm/cm Grade Count:5
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled". Each property range of values reported i..
Linear Mold Shrinkage 0.000600 - 0.0130 cm/cm
0.000600 - 0.0130 in/in
Average value: 0.00759 cm/cm Grade Count:23
Overview of materials for Silicone, RTV, Adhesive/Sealant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, RTV, Adhesive/Sealant Grade". Each property range of values reported is minimum and maximum va..
Linear Mold Shrinkage 0.0000900 - 0.0130 cm/cm
0.0000900 - 0.0130 in/in
Average value: 0.00459 cm/cm Grade Count:164
Overview of materials for Polysulfone (PSU)
This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Linear Mold Shrinkage 0.00100 - 0.0130 cm/cm
0.00100 - 0.0130 in/in
Average value: 0.00408 cm/cm Grade Count:26
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..
Linear Mold Shrinkage 0.000500 - 0.0130 cm/cm
0.000500 - 0.0130 in/in
Average value: 0.00447 cm/cm Grade Count:37
Overview of materials for Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 10% Glass Fiber Filler". Specific grades with glass content between 5% ..
Linear Mold Shrinkage -0.000500 - 0.0130 cm/cm
-0.000500 - 0.0130 in/in
Average value: 0.00732 cm/cm Grade Count:22
Overview of materials for Melamine-Phenolic Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Melamine-Phenolic Copolymer". Each property range of values reported is minimum and maximum values of ap..
Linear Mold Shrinkage 0.0100 - 0.0130 cm/cm

@Temperature 150 - 150 °C
0.0100 - 0.0130 in/in

@Temperature 302 - 302 °F
Average value: 0.0109 cm/cm Grade Count:17
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..
Linear Mold Shrinkage 0.0100 - 0.0130 cm/cm

@Time 900 - 900 sec
0.0100 - 0.0130 in/in

@Time 0.250 - 0.250 hour
Average value: 0.0109 cm/cm Grade Count:17
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..
Linear Mold Shrinkage 0.00400 - 0.0130 cm/cm
0.00400 - 0.0130 in/in
Average value: 0.00840 cm/cm Grade Count:25
Overview of materials for Polypropylene with 30% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Mica Filler". Specific grades with primary filler content between 25% and 34% are..
Linear Mold Shrinkage 0.00400 - 0.0130 cm/cm
0.00400 - 0.0130 in/in
Average value: 0.00719 cm/cm Grade Count:24
Overview of materials for Polypropylene with 40% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are..