Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.000800 - 0.00800 cm/cm | 0.000800 - 0.00800 in/in | Average value: 0.00547 cm/cm Grade Count:7 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00530 cm/cm Grade Count:54 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Linear Mold Shrinkage | 0.00500 - 0.00800 cm/cm | 0.00500 - 0.00800 in/in | Average value: 0.00628 cm/cm Grade Count:15 |
Overview of materials for Polycarbonate, Gamma Radiation Resistant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Gamma Radiation Resistant". Each property range of values reported is minimum and maximum.. |
|||
Linear Mold Shrinkage | -0.00100 - 0.00800 cm/cm | -0.00100 - 0.00800 in/in | Average value: 0.00220 cm/cm Grade Count:107 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00455 cm/cm Grade Count:174 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00420 cm/cm Grade Count:10 |
Overview of materials for Acrylic, High Flow, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, High Flow, Molded". Each property range of values reported is minimum and maximum values of app.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00800 cm/cm | 0.00100 - 0.00800 in/in | Average value: 0.00319 cm/cm Grade Count:7 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00800 cm/cm | 0.00400 - 0.00800 in/in | Average value: 0.00583 cm/cm Grade Count:4 |
Overview of materials for Nylon 11 with 10% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are includ.. |
|||
Linear Mold Shrinkage | 0.000200 - 0.00800 cm/cm | 0.000200 - 0.00800 in/in | Average value: 0.00255 cm/cm Grade Count:21 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00800 cm/cm @Thickness 3.20 mm |
0.00400 - 0.00800 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 1499 P X 125056 B Polyphenyl Sulfone (PPSU) Stainless Steel Fiber - EMI/RFI Shielding |
|||
Linear Mold Shrinkage | 0.00400 - 0.00800 cm/cm @Thickness 3.20 mm |
0.00400 - 0.00800 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 202 TFE 13 SI 2 Nylon 6/6 (PA) Glass Fiber - PTFE Lubricated - Silicone Lubricated |
|||
Linear Mold Shrinkage | 0.00500 - 0.00800 cm/cm @Thickness 3.20 mm |
0.00500 - 0.00800 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 300 FR Polycarbonate (PC), Unreinforced - Flame Retardant - UL94 V-0 The RTP 300 series of flame retardant materials offer dimensional stability, rigidity, heat resistance and ignition resistance. RTP 300 FR possesses a UL94 5V-A certification. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00800 cm/cm @Thickness 3.20 mm |
0.00300 - 0.00800 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 300 HF TFE 15 Polycarbonate (PC), PTFE Lubricated - High Flow |
|||
Linear Mold Shrinkage | 0.00100 - 0.00800 cm/cm | 0.00100 - 0.00800 in/in | Average value: 0.00436 cm/cm Grade Count:14 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00800 cm/cm | 0.00100 - 0.00800 in/in | Average value: 0.00313 cm/cm Grade Count:9 |
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Glass Fiber Filler". Each property range of values reported is minimum and .. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00800 cm/cm | 0.00100 - 0.00800 in/in | Average value: 0.00467 cm/cm Grade Count:19 |
Overview of materials for Polyethersulfone (PES), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% a.. |
|||
Linear Mold Shrinkage | 0.00100 - 0.00800 cm/cm | 0.00100 - 0.00800 in/in | Average value: 0.00335 cm/cm Grade Count:27 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Linear Mold Shrinkage | 0.00150 - 0.00800 cm/cm | 0.00150 - 0.00800 in/in | Average value: 0.00526 cm/cm Grade Count:248 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00800 cm/cm | 0.00300 - 0.00800 in/in | Average value: 0.00537 cm/cm Grade Count:18 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00468 cm/cm Grade Count:11 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00500 cm/cm Grade Count:8 |
Overview of materials for Acrylic, UV Stabilized, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, UV Stabilized, Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage | 0.00400 - 0.00800 cm/cm @Thickness 3.17 mm |
0.00400 - 0.00800 in/in @Thickness 0.125 in |
ASTM D955 |
RTP Company RTP 1002 TFE 15 Z Polybutylene Terephthalate (PBT), Glass Fiber Reinforced - PTFE Lubricated - FDA Compliant Ingredients |
|||
Linear Mold Shrinkage | 0.00600 - 0.00800 cm/cm @Thickness 3.20 mm |
0.00600 - 0.00800 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 2099 X 138762 PC/PBT Alloy ESD Protection - Permanently Static Dissipative - Impact Modified - UV Stabilized This compound has been formulated to meet the static dissipative requirements of the ATEX Directive. |
|||
Linear Mold Shrinkage | 0.00600 - 0.00800 cm/cm @Thickness 3.20 mm |
0.00600 - 0.00800 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 399 X 115062 G Polycarbonate (PC); Carbon Nanotube - Electrically Conductive - ESD Protection |
|||
Linear Mold Shrinkage | 0.00250 - 0.00800 cm/cm | 0.00250 - 0.00800 in/in | Average value: 0.00517 cm/cm Grade Count:75 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |
|||
Linear Mold Shrinkage | 0.00150 - 0.00800 cm/cm | 0.00150 - 0.00800 in/in | Average value: 0.00356 cm/cm Grade Count:13 |
Overview of materials for Polysulfone, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are inc.. |
|||
Linear Mold Shrinkage | 0.00200 - 0.00800 cm/cm | 0.00200 - 0.00800 in/in | Average value: 0.00420 cm/cm Grade Count:130 |
Overview of materials for Acrylic, Optical Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage | 0.00300 - 0.00800 cm/cm | 0.00300 - 0.00800 in/in | Average value: 0.00543 cm/cm Grade Count:7 |
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim.. |
|||
Linear Mold Shrinkage | 0.00500 - 0.00800 cm/cm @Thickness 3.20 mm |
0.00500 - 0.00800 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 2099 X 137399 A NS Polyester Alloy Flame Retardant - UV Stabilized - Medical Cleaner Resistant - No Subs |
|||
Linear Mold Shrinkage | 0.00600 - 0.00800 cm/cm @Thickness 3.20 mm |
0.00600 - 0.00800 in/in @Thickness 0.126 in |
ASTM D 955 |
RTP Company RTP 2099 X 138762 H PC/PBT Alloy Permanently Static Dissipative - ESD Protection - Impact Modified - UV Stabilized This compound has been formulated to meet the static dissipative requirements of the ATEX Directive. |