Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00700 - 0.0180 cm/cm
0.00700 - 0.0180 in/in
Average value: 0.0108 cm/cm Grade Count:24
Overview of materials for Polyetheretherketone, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value..
Linear Mold Shrinkage 0.00300 - 0.0180 cm/cm
0.00300 - 0.0180 in/in
Average value: 0.0102 cm/cm Grade Count:24
Overview of materials for Acetal Homopolymer, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Glass Fiber Reinforced". Each property range of values reported is minimum and maxim..
Linear Mold Shrinkage 0.00100 - 0.0180 cm/cm
0.00100 - 0.0180 in/in
Average value: 0.00669 cm/cm Grade Count:113
Overview of materials for Polycarbonate/PET Polyester Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values..
Linear Mold Shrinkage 0.00100 - 0.0180 cm/cm
0.00100 - 0.0180 in/in
Average value: 0.00743 cm/cm Grade Count:56
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
Linear Mold Shrinkage 0.00100 - 0.0180 cm/cm
0.00100 - 0.0180 in/in
Average value: 0.00226 cm/cm Grade Count:36
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 40% Glass Fiber Reinforced". Specific grades with glass content between 35% and 44% are incl..
Linear Mold Shrinkage 0.00100 - 0.0180 cm/cm
0.00100 - 0.0180 in/in
Average value: 0.00481 cm/cm Grade Count:51
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc..
Linear Mold Shrinkage 0.000500 - 0.0180 cm/cm
0.000500 - 0.0180 in/in
Average value: 0.00327 cm/cm Grade Count:31
Overview of materials for Nylon 66, 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in..
Linear Mold Shrinkage 0.00400 - 0.0180 cm/cm
0.00400 - 0.0180 in/in
Average value: 0.0126 cm/cm Grade Count:4
Overview of materials for Nylon 11, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Linear Mold Shrinkage 0.0100 - 0.0180 cm/cm
0.0100 - 0.0180 in/in
Average value: 0.0120 cm/cm Grade Count:33
Overview of materials for PVC, Wire and Cable Grade
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr..
Linear Mold Shrinkage 0.00600 - 0.0180 cm/cm
0.00600 - 0.0180 in/in
Average value: 0.0100 cm/cm Grade Count:9
Overview of materials for Ionomer, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma..