Physical Properties Metric English Comments
Density 1.16 - 1.42 g/cc

@Temperature 200 - 215 °C
0.0419 - 0.0513 lb/in³

@Temperature 392 - 419 °F
Average value: 1.22 g/cc Grade Count:16
Overview of materials for Acetal Homopolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values ..
Density 1.26 - 1.42 g/cc
0.0455 - 0.0513 lb/in³
Average value: 1.37 g/cc Grade Count:43
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m..
Density 1.18 - 1.42 g/cc
0.0426 - 0.0513 lb/in³
Average value: 1.32 g/cc Grade Count:27
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu..
Density 1.19 - 1.42 g/cc

@Temperature 250 - 250 °C
0.0430 - 0.0513 lb/in³

@Temperature 482 - 482 °F
Average value: 1.31 g/cc Grade Count:4
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..
Density 1.10 - 1.42 g/cc
0.0397 - 0.0513 lb/in³
Average value: 1.26 g/cc Grade Count:4
Overview of materials for Nylon 11 with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are includ..
Density 1.35 - 1.42 g/cc
0.0488 - 0.0513 lb/in³
Average value: 1.38 g/cc Grade Count:4
Overview of materials for Nylon 11 with 40% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 40% Glass Fiber Filler". Specific grades with glass content between 35% and 44% are includ..
Density 1.38 - 1.42 g/cc
0.0499 - 0.0513 lb/in³
ISO R 1184
Fainplast Compounds RI 059/1 Rigid PVC, Injection Molding
Fittings high fluidity
Density 1.38 - 1.42 g/cc
0.0499 - 0.0513 lb/in³
ISO R 1184
Fainplast Compounds RI 50 Rigid PVC, Injection Molding
Technical items
Density 1.34 - 1.42 g/cc
0.0484 - 0.0513 lb/in³
ASTM D792
Solvay Specialty Polymers Radel® R-7700 Polyphenylsulfone (PPSU)
Radel® R-7700 polyphenylsulfone sheet was developed specifically for aircraft interior applications. Through the use of a proprietary flame retardant package, this resin offers low heat release, ..
Density 1.38 - 1.42 g/cc
0.0499 - 0.0513 lb/in³
ISO R 1183
Fainplast Compounds CL 74 Flexible PVC, Sheathing
Mineral oil resistent
Density 1.38 - 1.42 g/cc
0.0499 - 0.0513 lb/in³
ISO R 1183
Fainplast Compounds FR 79 Flexible PVC, Insulation
Low temperatures
Density 1.38 - 1.42 g/cc
0.0499 - 0.0513 lb/in³
ISO R 1183
Fainplast Compounds GA 63 Flexible PVC, Flame Retardant Sheathing
Good flexibility
Density 1.38 - 1.42 g/cc
0.0499 - 0.0513 lb/in³
ISO R 1183
Fainplast Compounds GK 80/R Flexible PVC, Flame Retardant Sheathing Lead Free
Minearl oil resistant
Density 1.38 - 1.42 g/cc
0.0499 - 0.0513 lb/in³
ISO R 1184
Fainplast Compounds GS 77 Flexible PVC, Electrical Plugs
Plugs
Density 1.38 - 1.42 g/cc
0.0499 - 0.0513 lb/in³
ISO R 1183
Fainplast Compounds GS 77 Flexible PVC, Injection Molding for Technical Items
Plugs
Density 1.38 - 1.42 g/cc
0.0499 - 0.0513 lb/in³
ISO R 1183
Fainplast Compounds PMS 96 Flexible PVC, Extrusion
Semi-rigid adhesive profiles
Density 1.38 - 1.42 g/cc
0.0499 - 0.0513 lb/in³
ISO R 1184
Fainplast Compounds KL 77 Flexible PVC, Insulation for High Temperatures Lead Free
Operating temperature 105°C
Density 1.38 - 1.42 g/cc
0.0499 - 0.0513 lb/in³
ISO R 1184
Fainplast Compounds KL 90/2 Flexible PVC, Insulation for High Temperatures Lead Free
Operatine temperature 105°C
Density 1.36 - 1.42 g/cc
0.0491 - 0.0513 lb/in³
Molding; IS 867-1963
Amity Thermosets ATM 144 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control pane..
Density 1.37 - 1.42 g/cc
0.0495 - 0.0513 lb/in³
Molding; IS 867-1963
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Compression Molded
Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft/medium flow Applications:Telecommuni..
Density 1.26 - 1.42 g/cc
0.0455 - 0.0515 lb/in³
Average value: 1.31 g/cc Grade Count:7
Overview of materials for Polycarbonate, Glass Fiber & Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber & Bead Filled". Each property range of values reported is minimum and maximum..
Density 1.38 - 1.42 g/cc
0.0499 - 0.0513 lb/in³
ISO R 1184
Fainplast Compounds RI 548/H Rigid PVC, Antishock Injection Molding
Electric antishock fittings
Density 1.38 - 1.42 g/cc
0.0499 - 0.0513 lb/in³
ISO R 1183
Fainplast Compounds CKL 93 Flexible PVC, Sheathing Lead Free
Sheathing automotive cables
Density 1.38 - 1.42 g/cc
0.0499 - 0.0513 lb/in³
ISO R 1183
Fainplast Compounds CL 62 Flexible PVC, Sheathing
Sheath various purposes good flexibility
Density 1.38 - 1.42 g/cc
0.0499 - 0.0513 lb/in³
ISO R 1183
Fainplast Compounds FKA 88/1 Flexible PVC, Flame Retardant Insulation Lead Free
Insulation low temperatures