Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Fainplast Compounds KL 90/2 Flexible PVC, Insulation for High Temperatures Lead Free

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds KL 90/2 Flexible PVC, Insulation for High Temperatures Lead Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Operatine temperature 105°C
Physical Properties Metric English Comments
Density 1.38 - 1.42 g/cc
0.0499 - 0.0513 lb/in³
ISO R 1184
Mechanical Properties Metric English Comments
Hardness, Shore A 88 - 92
88 - 92
ISO R 868
Tensile Strength at Break >= 18.0 MPa
>= 2610 psi
ISO R 527
Elongation at Break >= 280 %
>= 280 %
ISO R 527
Thermal Properties Metric English Comments
Oxygen Index 27.5 %
27.5 %
ISO 4589
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm

@Temperature 23.0 °C
1.00e+14 ohm-cm

@Temperature 73.4 °F
ASTM D257
Descriptive Properties Value Comments
Thermal Stability (minutes) 200
CEI 20-34/3-2
Users viewing this material also viewed the following: