Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Amity Thermosets ATM 144 Phenolic Molding Organic Filler, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic
Manufacturer Amity Thermosets
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Amity Thermosets ATM 144 Phenolic Molding Organic Filler, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Characteristics:Good mouldability Good mechanical strengthGood electrical insulationGood surface finishMedium thermal stabilityColor- black, brownSoft/medium flow Applications: Electric control panel parts Small electric meter covers & partsElectric accessories ( superior quality )Glossy handles & knobsToaster & electric appliance partsLamp holderToilet seatsCarbon brush holdersDecor items ( e.g. ash trays )Starter push buttonsSolenoid switch covers ( medium quality ) Kitchen equipment ( eg. mixer, dishwasher, ovens ) fittingsTerminal boards, etc.Information provided by Amity Thermosets Limited
Physical Properties Metric English Comments
Density 1.36 - 1.42 g/cc
0.0491 - 0.0513 lb/in³
Molding; IS 867-1963
Apparent Bulk Density 0.620 - 0.690 g/cc
0.0224 - 0.0249 lb/in³
IS 867-1963
Water Absorption 0.30 - 0.55 %
0.30 - 0.55 %
IS 13411-1993
Linear Mold Shrinkage 0.0070 - 0.0083 cm/cm
0.0070 - 0.0083 in/in
IS 13411-1992
Mechanical Properties Metric English Comments
Tensile Strength at Break 46.0 - 60.0 MPa
6670 - 8700 psi
5 mm/min.; IS 867-1963
Shear Strength 66.0 - 76.0 MPa
9570 - 11000 psi
2mm/min.; IS 867-1963
Izod Impact, Notched 0.280 - 0.420 J/cm
0.525 - 0.787 ft-lb/in
IS 13411-1992
Electrical Properties Metric English Comments
Volume Resistivity 3.2e+10 - 3.2e+11 ohm-cm
3.2e+10 - 3.2e+11 ohm-cm
IS 3396-1979
Surface Resistance 1.00e+10 - 3.16e+10 ohm
1.00e+10 - 3.16e+10 ohm
IS 3396-1979
Dielectric Strength 5.50 - 7.00 kV/mm

@Temperature 90.0 °C
140 - 178 kV/in

@Temperature 194 °F
IS 2584-1963
Processing Properties Metric English Comments
Mold Temperature 160 - 180 °C
320 - 356 °F
Injection Pressure 15.68 - 34.3 MPa
2274 - 4970 psi
Mold Pressure
Cure Time 0.333 - 0.417 min
0.00556 - 0.00694 hour
per mm
Shelf Life 12.0 Month
12.0 Month
10-25°C