Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 7.30 g/cc | 0.264 lb/in³ | |
Indium Corp. 4N Commercial Indium Metal Indium is a versatile metal with unique physical properties.Indium has one of the widest liquid temperature ranges of any metal.Indium has a low vapor pressure, making it ideal for high vacuum appli.. |
|||
Density | 7.30 g/cc | 0.264 lb/in³ | |
Indium Corp. 6N5 High Purity Indium Metal High purity Indium is used as the starting material in the manufacture of indium based group III-V such asIn/PIn/AsIn/SbIn/Ga/AsIn/Ga/As/P These compound semiconductors find use in ultra high effici.. |
|||
Density | 7.30 g/cc | 0.264 lb/in³ | |
Indium Corp. 6N5WCI High Purity Indium Metal High purity Indium is used as the starting material in the manufacture of indium based group III-V such asIn/PIn/AsIn/SbIn/Ga/AsIn/Ga/As/P These compound semiconductors find use in ultra high effici.. |
|||
Density | 7.32 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy 160 Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 7.30 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy 87 Indium-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 7.31 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy 88 Indium Solder Alloy Information Provided by Indium Corporation |
|||
Density | 7.31 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy 90 Indium Solder Alloy Information Provided by Indium Corporation |
|||
Density | 7.31 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy 91 Indium Solder Alloy Information Provided by Indium Corporation |
|||
Density | 7.31 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy® 244 99.3Sn/0.7Cu Lead-Free Solder Alloy Inexpensive. Alloy of choice for general wave solder assembly.Information provided by the manufacturer, Indium Corporation. |
|||
Density | 7.31 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy® 4 Pure Indium Solder Soft, ductile metal has good wettability on many surfaces including ceramics, glass and quartz. Deforms indefinitely under load and has no tendency to become brittle, making it valuable for cryogeni.. |
|||
Density | 7.30 g/cc | 0.264 lb/in³ | |
Indium Corp. Sn992 Pb-Free Soldering Alloy Sn992 Pb-Free solder is a low cost alternative to traditional SAC305. In addition to the lower cost, this cobalt- and bismuth-doped Sn/Cu alloy produces smoother, shinier joints and lower dross (in.. |
|||
Density | 7.30 g/cc | 0.264 lb/in³ | |
Indium Corp. Sn995 Cobalt-Doped, Pb-Free Soldering Alloy Sn995 Cobalt-Doped Pb-Free Soldering Alloy is a cobalt-doped Sn/Cu alloy that provides a low cost alternative to traditional SAC305. In addition to the lower cost, this cobalt- and bismuth-doped Sn.. |
|||
Density | 7.30 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy 1 Indium-Tin Solder Alloy Fair wettability on glass, quartz, and many ceramics. Good low temperature malleability. Compensates for some CTE mismatch. Low vapor pressureInformation Provided by Indium Corporation |
|||
Density | 7.32 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy 258 Tin Solder Alloy Information Provided by Indium Corporation |
|||
Density | 7.30 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy® 1E In-Sn Solder Alloy Lowest melting point practical solder. Indium-tin eutectic with sharp melting point. Has good wettability on glass, quartz and many ceramics. Has good low temperature malleability and therefore com.. |
|||
Density | 7.30 g/cc | 0.264 lb/in³ | |
United Cast Bar Unibar 300 Continuously Cast Iron Unibar 300 is alloyed to achieve the properties, giving excellent wear resistance, strength & heat-treatment response, while still possessing reasonable machinability and an excellent surface finish.. |
|||
Density | 7.30 g/cc | 0.264 lb/in³ | |
United Cast Bar Unibar 400-15 As Cast Continuously Cast Spheroidal Graphite Iron Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend.. |
|||
Density | 7.30 g/cc | 0.264 lb/in³ | |
United Cast Bar Unibar 400-15 Fully Annealed Continuously Cast Spheroidal Graphite Iron Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend.. |
|||
Density | 7.30 g/cc | 0.264 lb/in³ | |
United Cast Bar Unibar 500-7 Continuously Cast Spheroidal Graphite Iron Offers higher wear resistance, strength & heat-treatment response while still possessing good machinability and excellent surface finishes. Noise and vibration damping are good in this grade.Unibar .. |
|||
Density | 7.30 g/cc | 0.264 lb/in³ | |
United Cast Bar Unibar 700-2 Continuously Cast Spheroidal Graphite Iron Offers higher wear resistance; strength & heat-treatment response while still possessing reasonable machinability and excellent surface finish. Noise and vibration damping are good in this grade.Uni.. |
|||
Density | 7.30 g/cc | 0.264 lb/in³ | |
Williams Advanced Alloys WS118 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 7.30 g/cc | 0.264 lb/in³ | |
Williams Advanced Alloys WS145 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 7.31 g/cc | 0.264 lb/in³ | |
Williams Advanced Alloys WS157 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 7.31 g/cc | 0.264 lb/in³ | |
American Elements Indium Nanoparticles General DescriptionIndium (In) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal nanostructure particles. Nanoscale Indium Particles are typically 20-40 nanomete.. |
|||
Density | 7.31 g/cc | 0.264 lb/in³ | |
California Fine Wire Stablohm 750 Chromium, Aluminum, and Iron Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 7.30 g/cc | 0.264 lb/in³ | |
AIM 52In/48Sn Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Density | 7.30 g/cc | 0.264 lb/in³ | |
AIM CASTIN Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Density | 7.30 g/cc | 0.264 lb/in³ | |
Alliance A-5 Alnico Magnetic Material |
|||
Density | 7.31 g/cc | 0.264 lb/in³ | |
Indium Corp. Indalloy 225 Indium Solder Alloy Information Provided by Indium Corporation |