Material Notes:
Offers higher wear resistance, strength & heat-treatment response while still possessing good machinability and excellent surface finishes. Noise and vibration damping are good in this grade.Unibar 500-7 can be hardened by conventional methods.Information provided by United Cast Bar Ltd.
Physical Properties Metric English Comments
Density 7.30 g/cc
0.264 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 170 - 230

@Load 3000 kg
170 - 230

@Load 6610 lb
10 mm ball
Tensile Strength 420 MPa

@Diameter 105 - 200 mm
60900 psi

@Diameter 4.13 - 7.87 in
420 MPa

@Diameter 205 - 600 mm
60900 psi

@Diameter 8.07 - 23.6 in
450 MPa

@Diameter 55.0 - 100 mm
65300 psi

@Diameter 2.17 - 3.94 in
500 MPa

@Diameter 25.0 - 50.0 mm
72500 psi

@Diameter 0.984 - 1.97 in
Tensile Stress 290 MPa

@Diameter 105 - 200 mm,
Strain 0.200 %
42100 psi

@Diameter 4.13 - 7.87 in,
Strain 0.200 %
290 MPa

@Diameter 205 - 600 mm,
Strain 0.200 %
42100 psi

@Diameter 8.07 - 23.6 in,
Strain 0.200 %
300 MPa

@Diameter 55.0 - 100 mm,
Strain 0.200 %
43500 psi

@Diameter 2.17 - 3.94 in,
Strain 0.200 %
320 MPa

@Diameter 25.0 - 50.0 mm,
Strain 0.200 %
46400 psi

@Diameter 0.984 - 1.97 in,
Strain 0.200 %
Elongation at Break 5.0 %

@Thickness 105 - 200 mm
5.0 %

@Thickness 4.13 - 7.87 in
5.0 %

@Thickness 205 - 600 mm
5.0 %

@Thickness 8.07 - 23.6 in
7.0 %

@Thickness 25.0 - 50.0 mm
7.0 %

@Thickness 0.984 - 1.97 in
7.0 %

@Thickness 55.0 - 100 mm
7.0 %

@Thickness 2.17 - 3.94 in
Component Elements Properties Metric English Comments
Carbon, C 3.25 - 3.7 %
3.25 - 3.7 %
Iron, Fe 92.83 - 94.19 %
92.83 - 94.19 %
as balance
Magnesium, Mg 0.040 - 0.070 %
0.040 - 0.070 %
Manganese, Mn 0.10 - 0.30 %
0.10 - 0.30 %
Phosphorous, P 0.015 - 0.080 %
0.015 - 0.080 %
Silicon, Si 2.4 - 3.0 %
2.4 - 3.0 %
Sulfur, S 0.0050 - 0.020 %
0.0050 - 0.020 %
Users viewing this material also viewed the following: