Indium Corp. Indalloy® 1E In-Sn Solder Alloy

Category Metal , Nonferrous Metal , Indium Alloy , Solder/Braze Alloy , Tin Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 1E In-Sn Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lowest melting point practical solder. Indium-tin eutectic with sharp melting point. Has good wettability on glass, quartz and many ceramics. Has good low temperature malleability and therefore compensates for some difference in coefficient of expansion when dissimilar materials are soldered.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 7.30 g/cc
0.264 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 4.5

@Load 100 kg,
Time 30.0 sec
4.5

@Load 220 lb,
Time 0.00833 hour
Tensile Strength, Ultimate 11.9 MPa
1730 psi
Elongation at Break 83 %
83 %
Shear Strength 11.2 MPa
1620 psi
Shear Bond Holding Strength
Thermal Properties Metric English Comments
CTE, linear 20.0 µm/m-°C

@Temperature 20.0 °C
11.1 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 34.0 W/m-K

@Temperature 85.0 °C
236 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 118 °C
244 °F
Eutectic
Solidus 118 °C
244 °F
Liquidus 118 °C
244 °F
Component Elements Properties Metric English Comments
Indium, In 52 %
52 %
Tin, Sn 48 %
48 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000150 ohm-cm
0.0000150 ohm-cm