Indium Corp. Indalloy® 244 99.3Sn/0.7Cu Lead-Free Solder Alloy

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 244 99.3Sn/0.7Cu Lead-Free Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Inexpensive. Alloy of choice for general wave solder assembly.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 7.31 g/cc
0.264 lb/in³
Thermal Properties Metric English Comments
Melting Point 227 °C
441 °F
Eutectic
Solidus 227 °C
441 °F
Eutectic
Liquidus 227 °C
441 °F
Eutectic
Component Elements Properties Metric English Comments
Copper, Cu 0.70 %
0.70 %
Tin, Sn 99.3 %
99.3 %