Material Notes:
Fair wettability on glass, quartz, and many ceramics. Good low temperature malleability. Compensates for some CTE mismatch. Low vapor pressureInformation Provided by Indium Corporation
Physical Properties Metric English Comments
Density 7.30 g/cc
0.264 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 4.5

@Load 100 kg,
Time 30.0 sec
4.5

@Load 220 lb,
Time 0.00833 hour
Tensile Strength at Break 11.9 MPa
1720 psi
Elongation at Break 83 %
83 %
Shear Strength 11.2 MPa
1630 psi
Thermal Properties Metric English Comments
CTE, linear 20.0 µm/m-°C

@Temperature 20.0 °C
11.1 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 34.0 W/m-K

@Temperature 85.0 °C
236 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 118 - 125 °C
244 - 257 °F
Solidus 118 °C
244 °F
Liquidus 125 °C
257 °F
Component Elements Properties Metric English Comments
Indium, In 50 %
50 %
Tin, Sn 50 %
50 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000147 ohm-cm
0.0000147 ohm-cm