Material Notes:
Sn992 Pb-Free solder is a low cost alternative to traditional SAC305. In addition to the lower cost, this cobalt- and bismuth-doped Sn/Cu alloy produces smoother, shinier joints and lower dross (in wave soldering) than SAC305 and other Sn/Cu based alloysFeaturesProduces shiny, smooth solder joints under most soldering conditionsLow cost - does not contain AgLower dross formation than other SAC and Sn/Cu-based alloysLess copper erosion than SAC305Compatible with other Sn/Cu-based alloys - no need to dump the potOptimized for use in solder paste form through the addition of BiPhysical Properties Time Above Liquidus: 30 to 90 secondsInformation provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Density 7.30 g/cc
0.264 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength 28.0 MPa
4060 psi
Thermal Properties Metric English Comments
Melting Point 227 °C
441 °F
Descriptive Properties Value Comments
Peak Temperature 237° - 255°C