Williams Advanced Alloys WS145 Solder

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy
Manufacturer Williams Advanced Alloys
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Williams Advanced Alloys WS145 Solder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Physical Properties Metric English Comments
Density 7.30 g/cc
0.264 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 40.7 MPa
5900 psi
Thermal Properties Metric English Comments
CTE, linear 31.0 µm/m-°C

@Temperature 20.0 °C
17.2 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 33.0 W/m-K
229 BTU-in/hr-ft²-°F
Melting Point 118 - 145 °C
244 - 293 °F
Solidus 118 °C
244 °F
Liquidus 145 °C
293 °F
Component Elements Properties Metric English Comments
Indium, In 42 %
42 %
Tin, Sn 58 %
58 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00001536 ohm-cm
0.00001536 ohm-cm