Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 7.31 g/cc
0.264 lb/in³
Thermal Properties Metric English Comments
Melting Point 143 - 151 °C
289 - 304 °F
Solidus 143 °C
289 °F
Liquidus 151 °C
304 °F
Component Elements Properties Metric English Comments
Indium, In 90 %
90 %
Tin, Sn 10 %
10 %