Material Notes:
Soft, ductile metal has good wettability on many surfaces including ceramics, glass and quartz. Deforms indefinitely under load and has no tendency to become brittle, making it valuable for cryogenic applications.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 7.31 g/cc
0.264 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 0.90
0.90
Tensile Strength, Ultimate 1.90 MPa
276 psi
Elongation at Break 22 - 41 %
22 - 41 %
Modulus of Elasticity 10.8 GPa
1570 ksi
Shear Strength 6.10 MPa
885 psi
Shear Bond Holding Strength
Thermal Properties Metric English Comments
Heat of Fusion 28.47 J/g
12.25 BTU/lb
CTE, linear 29.0 µm/m-°C

@Temperature 20.0 °C
16.1 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.243 J/g-°C
0.0581 BTU/lb-°F
Solid
Thermal Conductivity 86.0 W/m-K

@Temperature 85.0 °C
597 BTU-in/hr-ft²-°F

@Temperature 185 °F
Melting Point 157 °C
315 °F
Solidus 157 °C
315 °F
Liquidus 157 °C
315 °F
Component Elements Properties Metric English Comments
Indium, In 100 %
100 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000720 ohm-cm
0.00000720 ohm-cm