Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Multibase Multi-Pro® 7518 C Natural Polypropylene Unspecified filler/ reinforcment, 75% by weight.Forms:PelletsInformation provided by Multibase |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Covestro Petlon® DP3-1018 Semi-Crystalline PET, 35% Mineral/Glass Fiber
(discontinued **) Characteristics: Flame Retardant: Good Processability, Low Warpage, High RigidityApplications: Appliance, Telecommunication and Electrical HousingsProcessing: Injection Molding (Melt Temperature: 49.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Plenco 50045 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 50045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is UL listed and available in white, natural, and black.Information s.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ixef® 2030 Polyarylamide (PARA)
(Unverified Data**) Ixef 2030 is a 55% glass-fiber/mineral reinforced polyarylamide compound which exhibits high strength, very high stiffness, low warpage, excellent creep resistance and outstanding surface gloss. - B.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | |
LATI Latamid 6 H2 G/65 PA 6, 65% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | |
LATI Later 4 G/50 PBT, 50% Glass Fiber Reinforced Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP RFL369 PA6.6 (Europe-Africa-Middle East) LNP* LUBRICOMP* RFL369 is a compound based on PA 66 resin containing Glass Fiber, PTFE, Flame Retardant. Added features include: Flame Retardant, internally lubricated |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | |
SGL Carbon Group Ridurid® EK 60 High Performance Graphite Filled Plastic Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Ixef® 2030 Polyarylamide (PARA), 55% GlassMineral Ixef® 2030 is a 55% glass-fiber/mineral reinforced polyarylamide compound which exhibits high strength, very high stiffness, low warpage, excellent creep resistance and outstanding surface gloss... |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp RX06423 PA 66 LNP* Thermocomp* RX06423 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized.This data was supplied b.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp RX06423 PA 66 LNP* Thermocomp* RX06423 is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized.This data was supplied b.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp 2C004 LNP THERMOCOMP* 2C004 is a compound based on Ethylene Tetrafluoroethylene Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was sup.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | |
UCAR Carbon UCAR® CS Extruded Graphite Densified prior to graphitization, Grade CS is an extruded graphite 25-30% higher in strength than CBY. Grade CS is a low ash graphite with an oxidation resistance similar to grade CBY. It is the ma.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Westlake Plastics Kynar® PVDF CN-P Polyvinylidene Fluoride (conductive) Carbon-powder-filled, thermally stable, conductive material with consistent resistivities |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Zeus EFEP Tubing |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | |
Loctite® 3565 High performance epoxy, high Tg and low CTE High Tg Underfill COB/DCA Encapsulants are essential to the reliability of flip chip assemblies because they minimize the thermal mismatch between the flip chip and substrate.Loctite® Underfills and Encapsulants imp.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | |
Cosmic Plastics D45 Mineral Filled Ortho Diallyl Phthalate Molding Compound Data provided by the manufacturer. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Unitika UNILATE® 1 NC PET Flame resisting gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, a.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Ensinger Tecatron® XP-78 Compression Molded PPS Compound, 47% PTFE Filled Seal Material Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ASTM D792 |
Applied Composites 175 Vinylester SMC Industry Application: TransportationProduct Application: Structural ExteriorDistinct Features: Limited PigmentabilityInformation provided by Applied Composites Corporation. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | |
A. Schulman ComAlloy Voloy® 431 Glass/Mineral Reinforced, PET Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.74 g/cc | 0.0629 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP 2X04505 ETFE LNP* THERMOCOMP* 2X04505 is a compound based on ETFE resin containing Proprietary Filler(s). |