Applied Composites 175 Vinylester SMC

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Vinyl Ester , Vinyl Ester Sheet Molding Compound
Manufacturer Applied Composites Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Applied Composites 175 Vinylester SMC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Industry Application: TransportationProduct Application: Structural ExteriorDistinct Features: Limited PigmentabilityInformation provided by Applied Composites Corporation.
Physical Properties Metric English Comments
Density 1.74 g/cc
0.0629 lb/in³
ASTM D792
Water Absorption 0.12 %
0.12 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 115
115
ASTM D785
Tensile Strength, Ultimate 221 MPa
32000 psi
ASTM D638
Flexural Strength 386 MPa
56000 psi
ASTM D790
Flexural Modulus 15.2 GPa
2200 ksi
Tangent; ASTM D790
Taber Abrasion, mg/1000 Cycles 1.0
1.0
% Loss 1000 Cycles; FTMS1091
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 204 °C
>= 400 °F
Flexural Load; ASTM D648