Category Polymer , Thermoplastic , Fluoropolymer , PVDF , Polyvinylidinefluoride (PVDF), Molded/Extruded
Manufacturer Westlake Plastics
Trade Name KYNAR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Plastics Kynar® PVDF CN-P Polyvinylidene Fluoride (conductive).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Carbon-powder-filled, thermally stable, conductive material with consistent resistivities
Physical Properties Metric English Comments
Density 1.74 g/cc
0.0629 lb/in³
ASTM D792
Water Absorption <= 0.060 %
<= 0.060 %
ASTM D570; 24 hrs.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.9 MPa
5200 psi
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Flexural Strength 44.8 MPa
6500 psi
ASTM D790
Flexural Modulus 0.931 GPa
135 ksi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 56.1 °C
133 °F
ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity <= 1e+05
<= 1e+05
Dry; ASTM D257
Surface Resistance <= 1e+05
<= 1e+05
Dry; ASTM D257